Welding of A182 F22 material to SS 347

Materials Science, Metallurgy, Welding, NDTs, Reliability Assessment, Failure Analysis, etc.
Post Reply
arcpro
Posts: 356
Joined: 16 Apr 2010, 18:46
Area of interest: Manufacturing Engineering

Welding of A182 F22 material to SS 347

Post by arcpro »

We have to weld a flange of A182 F22 material to SS 347 pipe. Please guide.
ashfaqanwer
Site Admin
Posts: 443
Joined: 16 Mar 2010, 03:36

Re: Welding of A182 F22 material to SS 347

Post by ashfaqanwer »

Where buttering is not possible:
1. Preheat F22 side at 200 C
2. Weld with ER/E-309L and heat treat the joint when its above 12.7 mm thickness

Where buttering is possible:
1. Preheat F22 side at 200 C
2. Perform buttering on the F22 with ER-NiCr-3 (Inconel 82)
3. Heat treat after buttering at 750 C
4. Then weld with ER-NiCr-3 rods and E-NiCrFe-3 electrodes without preheating and post heating

Hope this would help.
Ashfaq Anwer
-PetroStreet.com
arcpro
Posts: 356
Joined: 16 Apr 2010, 18:46
Area of interest: Manufacturing Engineering

Re: Welding of A182 F22 material to SS 347

Post by arcpro »

Thanks.
arcpro
Posts: 356
Joined: 16 Apr 2010, 18:46
Area of interest: Manufacturing Engineering

Re: Welding of A182 F22 material to SS 347

Post by arcpro »

Ashfaq,
One more question coming in my mind is regarding heat treatment of weld in 309L as you mentioned.
There seem a possibility of sensitization of stainless steel, what do you say about this?
Post Reply